Finally, the third factor is application. It is important to consider time, temperature and pressure for a pressure sensitive adhesive. Acrylic pressure sensitive adhesives require a dwell time to flow out and achieve maximum peel strength. The surfaces should be at room temperature or above and only light contact pressure is required as long as air is not trapped in the interface (15 pounds per square inch for flexible to rigid and flexible to flexible for 5 seconds).